49 CFR § 192.489 Transportation of Natural and Other Gas by Pipeline: Minimum Federal Safety Standards

§ 192.489 Remedial measures: Cast iron and ductile iron pipelines.

Current through Sep 25, 2026 · Read all of Part 192

⚠ 31 pending changes to Part 192

(a) General graphitization. Each segment of cast iron or ductile iron pipe on which general graphitization is found to a degree where a fracture or any leakage might result, must be replaced.

(b) Localized graphitization. Each segment of cast iron or ductile iron pipe on which localized graphitization is found to a degree where any leakage might result, must be replaced or repaired, or sealed by internal sealing methods adequate to prevent or arrest any leakage.